We have more than 5000 clients in more than
We can help supply all of the ASTM A335 T11 ERW Pipe or linepipe supplies that your company needs for use in the oil or natural gas industries. High strength low alloy steel specifications for these pipes regulate usage for standard ASTM A335, ASTM A333 and ASTM A213 pipes. ASTM A335 T11 ERW Pipe is the part of ASTM A335, the pipe shall be suitable for bending, flanging, and similar forming operations, and for fusion welding.
All products are industry-standard conforming to or exceeding API, ASTM, ASME, ANSI and other national and international standards.
Chrome Moly pipe has become a standard in the power generation industry and the petro-chemical industry, not only because of its tensile strength, corrosion resistance and high-temperature strength, but also for its cost-effectiveness. Grades P-11, P-22 - P-91 & P-92 are prevalent grades for the power industry, while P-5 & P-9 are the major refinery processing grades utilized.
Pipes :- ASTM A335 GR P5 | GR P9 | GR P11 | P12 | GR P5 | GR T11 | P92.
Size Range: 1/2" - 24"
Schedules: 20, 30, 40, Standard (STD), 60, Extra Heavy (XS), 80, 100, 120, 140, 160, XXS
Tubes :- ASME SA213 Grade T11, T12, T11, T11, T11, T111, T112
Size Range: 12.7MM OD TO 168.7 MM OD
Thickness: 2MM TO 16MM THK
Chemical Requirements
Grade |
T-5 | T-9 | T-11 | T-22 | T-91 | T-91 shall also include the following: | |
Element | UNS Designation | K41545 | S50400 | K11597 | K21590 | K91560 | |
Carbon | 0.15 max | 0.15 max | 0.05 - 0.15 | 0.05 - 0.15 | 0.08 - 0.12 | V at 0.18 - 0.25 | |
Manganese | 0.30 - 0.60 | 0.30 - 0.60 | 0.30 - 0.60 | 0.30 - 0.60 | 0.30 - 0.60 | N at 0.030 - 0.070 | |
Phosphorous, max | 0.025 | 0.025 | 0.025 | 0.025 | 0.020 | Ni at 0.40 max | |
Sulfur, max | 0.025 | 0.025 | 0.025 | 0.025 | 0.010 | Al at 0.02 max | |
Silicon | 0.50 max | 0.25 - 1.00 | 0.50 - 1.00 | 0.50 max | 0.20 -0.50 | Cb at 0.06 - 0.10 | |
Chromium | 4.00 - 6.00 | 8.00 - 10.00 | 1.00 - 1.50 | 1.90 - 2.60 | 8.00 - 9.50 | Ti at 0.01 max | |
Molybdenum | 0.45 -0.65 | 0.90 - 1.10 | 0.44 - 0.65 | 0.87 - 1.13 | 0.85 - 1.05 | Zr at 0.01 max |
Physical Properties
P-5 | P-9 | P-11 | P-22 | P-91 | T11 shall not have a hardness not exceeding 250 HB/265 HV [25HRC]. | |
Tensile Strength, min., psi | ||||||
ksi | 60 | 60 | 60 | 60 | 85 | |
MPa | 415 | 415 | 415 | 415 | 585 | |
Yield Strength, min., psi | ||||||
ksi | 30 | 30 | 30 | 30 | 60 | |
MPa | 205 | 205 | 205 | 205 | 415 |
Physical Properties
P-5 | P-9 | P-11 | P-22 | P-91 | T11 shall not have a hardness not exceeding 250 HB/265 HV [25HRC]. | |
Tensile Strength, min., psi | ||||||
ksi | 60 | 60 | 60 | 60 | 85 | |
MPa | 415 | 415 | 415 | 415 | 585 | |
Yield Strength, min., psi | ||||||
ksi | 30 | 30 | 30 | 30 | 60 | |
MPa | 205 | 205 | 205 | 205 | 415 |
Russia, Algiers, Antananarivo, Mbuji-Mayi, Subra al-Haymah, Nairobi, Bulawayo, London, Fez, Algeria, Maiduguri, Giza, Port Elizabeth, New Zealand, Johannesburg, Indonesia, Italy, Colombo, Ghana, Mozambique, Colombia, Qatar, Argentina, Zaria, Pretoria, Freetown, Khartoum, South Africa, Lagos, Bahrain, Turkey, Australia, Angola, United States, Douala, Kampala, Luanda, Hong Kong, Azerbaijan, Conakry, Kuwait, Casablanca, Tunisia, Abu Dhabi, Houston, Peru, Ethiopa, Kolwezi, Kaduna, Oman, UK, Israel, Dar es Salaam, Mogadishu, Alexandria, Saudi Arabia, Accra, Kinshasa, Abidjan, Yemen, Africa, Cairo, Cameroon, Brazil, Chine, Venezuela, Vietnam, Ouagadougou, Iran, Brazzaville, Addis Ababa, Dubai, Jordan, Thailand (Bangkok), Trinidad and Tobago, Tripoli, Cape Town, Uganda, Cyprus, Nigeria, Soweto, New York, Democratic Republic of the Congo, Omdurman, Mexico, Morocco, Egypt, Singapore, Iraq, Sri Lanka, Bamako, Harare, Durban, Kazakhstan, Yaoundé, Lubumbashi, Maputo, Germany, Ibadan, Benin, Malaysia, UAE, Sudan, Rabat, Lebanon, Port Harcourt, Canada, Kano.
Bhiwadi, Abu Dhabi, Hyderabad, Suryapet, Yemen, Ghana, Tadepalligudem, Tripura, Durban, Subra al-Haymah, Rabat, India, Conakry, Benin, Maharashtra, Uganda, Miryalaguda, Cairo, Angola, Benin, Port Harcourt, Nairobi, Cameroon, Antananarivo, Freetown, Jaipur, Lucknow, Hong Kong, Pune, Casablanca, Mumbai, Mozambique, Zaria, Kolkata, Ethiopa, Mizoram, Singapore, Karnataka, Bulawayo, Algeria, Ballia, Dar es Salaam, Venezuela, Cyprus, Mogadishu, Colombo, Surat, Port Elizabeth, Tripoli, Abidjan, Oman, New York, Bundi, Lagos, Thailand (Bangkok), Kano, Kolwezi, Addis Ababa, Buxar, Soweto, Cape Town, Baraut, Udgir, Betul, Kinshasa, Fez, Lubumbashi, Alexandria, Kerala, Ibadan, Khartoum, Manipur, Nagapattinam, Douala, Sadar, Democratic Republic of the Congo, Algiers, Bansberia, Jamalpur, Kaduna, Mbuji-Mayi, Bangalore, Maiduguri, Jordan, Morocco, Harare, Qatar, Ahmedabad, Lebanon, Chennai, Luanda, Kampala, Russia, Dakar, Maputo, Yaoundé, Accra, Johannesburg, Andhra Pradesh, Giza, Omdurman, Ambala, Puducherry, Ouagadougou, Bamako, Pretoria, Brazzaville, Muktsar, Delhi.
Quality a335 pipes price list, alloy steel pipes price, a213 tubes price, alloy steel pipes specification, alloy pipe definition, p22 material composition, p22 pipe welding procedure, p22 material welding, astm a335 pdf, p22 material equivalent, p91 chemical composition, astm a335 p11, p91 material composition, p11, p22, p9 and p91 material, 9 chrome welding procedure, alloy steel pdf, steel alloy definition, astm a335 properties, astm a335 pipe, difference between p91 and p92 material, a213 tubing, chrome moly tubing suppliers, ASTM A335 Chrome Moly Pipe, a335 high pressure pipe Manufacturer, Supplier in India.